Organo Modified Clay: Advanced Rheological Solutions for Industrial Applications
What is Organo Modified Clay?
Organo modified clay, also known as organoclay or organophilic clay, is a high-efficiency rheological additive derived from sodium bentonite through advanced modification processes. This specialized material serves as a versatile thixotropic agent, anti-settling agent, and viscosity control agent across multiple industrial applications.
Key Properties
- Excellent thickening ability
- High thixotropic properties
- Superior suspension characteristics
- Anti-pigment sagging properties
Alternative Names
Technical Specifications
| Parameter | Specification |
|---|---|
| Composition | Organic derivative of montmorillonite clay |
| Appearance | Fine powder, light yellow to off-white |
| Moisture Content (105°C, 2hr) | ≤3.5% |
| Loss on Ignition (1000°C) | 34.7% |
| Bulk Density | 0.53g/cm³ |
| Fineness (<74μm, %) | ≥98% |
Industrial Applications
Paints & Coatings
- • Solvent-based automotive coatings
- • Marine and anti-corrosion coatings
- • High-temperature industrial coatings
- • Epoxy and polyurethane systems
- • Wood and metal protective coatings
Printing Inks
- • Gravure and flexographic inks
- • Screen printing inks
- • UV-curable ink systems
- • Packaging and industrial inks
- • Digital printing formulations
Grease & Lubricants
- • Mineral oil-based greases
- • Synthetic oil formulations
- • High-temperature applications
- • Vegetable oil-based systems
- • Complex lithium greases
Drilling Fluids
- • Oil-based drilling fluids
- • Invert emulsion systems
- • Completion and workover fluids
- • Synthetic base oil formulations
- • Low BTEX base oil systems
Product Grades & Classifications
Solvent-Based Grades
Water-Based Grades
Drilling Grades
Polarity Classification
Low Polarity
Hydrocarbon solvents
Medium Polarity
Aromatic solvents
High Polarity
Polar solvents
Usage Guidelines for Grease Applications
Required Materials
- • Organoclay dosage: 7-10% of total formulation
- • Polar activator: Acetone/water (95/5 ratio)
- • Activator dosage: 20-30% of organoclay weight (2-3% of total formulation)
Step-by-Step Process
-
1
Heat Base Oil
Heat base oil to 60-70°C if conditions permit
-
2
Add Organoclay
Add organoclay while stirring, stir for 5-10 minutes
-
3
Add Polar Activator
Add polar activator and other additives, stir for 25-30 minutes
-
4
Process
Use pump for colloid grinding and homogenization
-
5
Final Steps
Deair, filtrate, and pack the final product
Storage & Packaging
Storage Conditions
- Temperature: 0°C - 30°C
- Dry, well-ventilated area
- Keep container closed
- 24-month shelf life
Packaging Options
- • 25kg kraft bags
- • 50lb kraft bags
- • 600kg bulk bags
- • Custom packaging available
Container Loading:
20FCL: 15MT (with pallet) / 18MT (without pallet)
40FCL: 25.2MT (with pallet)
Why Choose CAMP-SHINNING Organo Modified Clay?
Industry Leadership
- • 20+ years of R&D experience
- • 20,000 tonnes annual capacity
- • 25% global market share
- • ISO9001 certified quality
Technical Excellence
- • Proprietary bentonite deposits
- • National patent certificate
- • Advanced testing equipment
- • Comprehensive quality traceability